Method for preparing bioceramic in complex phase of hydroxyapatite and beta triealcium phosphate |
Title: |
Method for preparing bioceramic in complex phase of hydroxyapatite and beta triealcium phosphate |
|
Application Number: |
200410030651 |
Application Date: |
2004/04/02 |
Announcement Date: |
2005/01/12 |
Pub. Date: |
|
Publication Number: |
1562873 |
Announcement Number: |
|
Grant Date: |
|
Granted Pub. Date: |
|
ApplicationType: |
Invention |
State/Country: |
11[China|beijing] |
IPC: |
A61F 2/28, A61K 6/04, C04B 35/447, C04B 35/626 |
Applicant(s): |
Tsinghua Univ. |
Inventor(s): |
Wang Chen, Dong Limin, Tian Jiemo |
Key Words: |
hydroxyapatite, beta triealcium phosphate, complex phase, bioceramic, preparing method |
Abstract: |
In the invention, biological glass powder (weight percentage is 5-15) is added in oxhydryl kietyoite powder to be formed by dry pressing on pressure 10-30 Mpa, then to be fired in temp. 1050-1250 deg.C to produce compound biological ceramics of oxhydryl kietyoite and beta-tricalcium phosphate that content can be controlled. |
Claim: |
|
Priority: |
|
PCT: |
|
LegalStatus: |
|