Pretrement of tail ore, concretion cementing material prepared therewith and their prepn |
Title: |
Pretrement of tail ore, concretion cementing material prepared therewith and their prepn |
|
Application Number: |
200610103677 |
Application Date: |
2006/07/28 |
Announcement Date: |
2007/01/03 |
Pub. Date: |
|
Publication Number: |
1887764 |
Announcement Number: |
|
Grant Date: |
|
Granted Pub. Date: |
|
ApplicationType: |
Invention |
State/Country: |
11[China|beijing] |
IPC: |
C04B 7/14, C04B 7/24 |
Applicant(s): |
Beijing Lanzi Concretion Sci-Tech Co., Ltd. |
Inventor(s): |
Sun Henghu, Ni Wen, Xu Yuefeng, Xu Weirui, Feng Xiangpeng, Yi Zhonglai |
Key Words: |
Pretrement of tail ore, concretion cementing material, preparation |
Abstract: |
The present invention relates to pre-treatment of tail ore, concretion cementing material obtained therewith and their preparation process. Tail ore in 30-90 wt%, salts connecting K+, Na+, Ca2+, Mg2+ and/or Fe2+ ion and acid radical ions in 0.1-8 wt%, and other material containing crystal water, hydroxide radical, hydroxyl group, CO22 or other volatile components in 5-60 wt% are mixed, and the mixture is then hydrothermal alteration reacted at 200-900 deg.c. Then, the hydrothermal alteration reacted material in 50-90 wt%, cement clinker in 0.1-29 wt%, blast furnace slag or other high temperature treated waste in 0-30 wt%, gypsum in 0-8 wt% and rock forming agent in 0.1-5 wt% are mixed and ground to obtain cement powder. The cement powder has high strength and high stability. |
Claim: |
|
Priority: |
|
PCT: |
|
LegalStatus: |
|
Relevancy information |
|
|
|
Other Patents of Same Inventor |
|
|
|
|
Last Update |
|
|
 |
2008-4-17 |
|
Selected patents owned by Tsinghua University filed in 2005 are loaded. |
 |
2008-3-31 |
|
Selected patents owned by Tsinghua University filed in 2006 and 2007 are load. |
|
|