Anticorrosion high-Mg low-Si aluminium alloy rich in Mn and Cr |
Title: |
Anticorrosion high-Mg low-Si aluminium alloy rich in Mn and Cr |
|
Application Number: |
02104339 |
Application Date: |
2002/03/01 |
Announcement Date: |
2002/12/04 |
Pub. Date: |
|
Publication Number: |
1382820 |
Announcement Number: |
1176237 |
Grant Date: |
2004-11-17 |
Granted Pub. Date: |
2004-11-17 |
ApplicationType: |
Invention |
State/Country: |
11[China|beijing] |
IPC: |
C22C 21/08 |
Applicant(s): |
Tsinghua Univ |
Inventor(s): |
Li Jianguo, Guo Daohua |
Key Words: |
Anticorrosion, high-Mg low-Si, aluminium alloy, Mn, Cr |
Abstract: |
An anticorrosion high-Mg low-Si Al-alloy rich in Mn and CR contains mg (0.6-1 wt.%), Si (0.2-0.6 wt.%), Mn (0.1-1 wt.%), Cr (0.1-0.4 wt.%), Fe (0-0.3 wt.%), Cu (0-0.2 wt.%), Zn (0-0.25 wt.%), and Al (rest). Its advantages are high anticorrosion and mechanical performance. |
Claim: |
|
Priority: |
|
PCT: |
|
LegalStatus: |
|
Relevancy information |
|
|
|
Other Patents of Same Inventor |
|
|
|
|
Last Update |
|
|
 |
2008-4-17 |
|
Selected patents owned by Tsinghua University filed in 2005 are loaded. |
 |
2008-3-31 |
|
Selected patents owned by Tsinghua University filed in 2006 and 2007 are load. |
|
|